Part A (polyol):
Specific Gravity, g/cm³ 1.14
Viscosity, Brookfield - RV, 25 °C, MPa·s (cP):
Spindle 6, speed 20 rpm 10, 000 to 30, 000
Part B:
Specific Gravity, g/cm³ 1.05
Viscosity, Brookfield - RVDV, 25 °C, MPa·s (cP):
Spindle 4, speed 20 rpm 3, 000 to 8, 000
TYPICAL CURING PERFORMANCE
Curing Properties
Cure Time @ 25 °C, hours 2
Gel Time @ 25 °C, minutes 7
TYPICAL PROPERTIES OF CURED MATERIAL
Cured @ 25 °C except where noted
Physical Properties:
Hardness (Shore A), ASTM D2240 87
Tensile Strength, ISO 37 N/mm² 11
(psi) 1, 600
Part A (polyol):
Specific Gravity, g/cm³ 1.14
Viscosity, Brookfield - RV, 25 °C, mPa@s (cP):
Spindle 6, speed 20 rpm 10,000 to 30,000
Part B:
Specific Gravity, g/cm³ 1.05
Viscosity, Brookfield - RVDV, 25 °C, mPa@s (cP):
Spindle 4, speed 20 rpm 3,000 to 8,000
TYPICAL CURING PERFORMANCE
Curing Properties
Cure Time @ 25 °C, hours 2
Gel Time @ 25 °C, minutes 7
TYPICAL PROPERTIES OF CURED MATERIAL
Cured @ 25 °C except where noted
Physical Properties:
Hardness (Shore A), ASTM D2240 87
Tensile Strength, ISO 37 N/mm² 11
(psi) 1,600